2D/1D cut plans, machine rates and signed quotes

How much wire and gas a foot of MIG weld really burns

Deposited metal comes from geometry: length times leg squared over two, plus reinforcement, times steel density. The wire you buy is that metal divided by deposition efficiency, and gas flows while the arc is on and at every start. The biggest line is the operating factor: at 30% arc-on time, every minute of welding takes more than three minutes of bench time.

Fillet weld (30 ft)Wire burnedC25 gasArc timeBench at 30%Cost / ft
1/8 in fillet, 1 pass0.95 lb12.9 cu ft25 min 43 s1 h 25 min$3.89
3/16 in fillet, 1 pass2.15 lb12.9 cu ft25 min 43 s1 h 25 min$4.00
1/4 in fillet, 2 passes3.81 lb25.7 cu ft51 min 26 s2 h 51 min$7.96
  1. Measure feet of weld per joint and the real fillet leg: going from 3/16 to 1/4 in multiplies deposited metal by 1.78.
  2. Divide deposited metal by deposition efficiency: about 92% for solid wire with C25 gas.
  3. Work out gas from arc time plus pre and post-flow at every start, and spread it over the cubic feet in the cylinder.
  4. Turn arc time into bench hours by dividing by the real operating factor of your shop, not the catalog figure.
Commercial quote, not a tax document

FAQ

What operating factor should a fab shop use?
Between 20 and 40% for manual MIG: the rest of the time goes to fit-up, tacking, spool changes and cleanup. Measure it for a week with the arc-on counter on the machine.
Do I charge wire by the pound or by the spool?
By the pound burned, because the spool keeps working on the next job. Charge a whole spool only for special wire you will not use again.